SN-16A

42
SAMWHA ELECTRONICS
Material Characteristics
Ni-Zn Material
Material
SN-16A
μiac
Initial permeability
Relative loss factor
1600 ±20%
tanδ/μiac
×10 25℃
25 (0.1MHz)
Saturation flux density (1194A/m)
Bs
mT
25℃
300
Remanence
Br
mT
25℃
120
Coercivity
Hc
A/m
25℃
15
Relative temp. factor (20℃∼60℃)
-6
×10 /℃
5∼10
Curie Temperature
Tc
℃
>130
Density
d
㎏/㎥
Resistivity
ρ
㏁·m
αμr
-6
5.0 ×103
25℃
>10
Note : 1) Typical values
2) The values were obtained with toroidal cores(30X8-20H) at room temperature unless indicated otherwise
Permeability vs. Frequency
Permeability vs. Temperature
2500
2000
2000
μ'
Initial permeability, μ iac
Complex permeability, μ',μ"
2500
1500
1000
μ"
500
0
100k
1M
1500
1000
500
0
10M
0
20
tan δ/μ i vs. Frequency
60
80
100
120
140
160
Bm vs. Hm
400
10
0
350
10-1
25℃
300
Bm(mT)
Relative loss factor, tan δ/μ i
40
Temperature (℃)
Frequency (Hz)
10-2
10-3
250
200
100℃
150
100
10-4
10-5
100k
50
0
1M
Frequency (MHz)
10M
0
200
400
600
Hm(A/m)
800
1000