Property
Test Method
Units
Value
ASTM D1238
ASTM D792
ASTM D570
g/10min
%
17~21
1.55
0.2
ASTM D1525
ASTM D648
℃
166
4.6kg/cm2 ( 0.45MPa )
℃
165
HDT/A 18.6kg/cm2 ( 1.81MPa )
Vicat Softening Temperature
℃
140
162
Physical
Melt Index
Specific Gravity
Water Absorption
23℃, Equilibrium 60%RH
Thermal
Melting Point
Heat Deflection Temperature
HDT/A
Coeff. Of Linear Thermal Expansion
Flammability
℃
ASTM D1525
ASTM D696
UL 94
x 10
-5
cm/cm·℃
5~7
HB
Mechanical
Tensile Strength
Tensile Elongation
23℃
23℃
ASTM D638
ASTM D638
kg/cm2 (MPa)
%
630 (62)
10
Flexural Strength
23℃
ASTM D790
kg/cm2 (MPa)
1200 (118)
23℃
23℃
M scale
ASTM D790
ASTM D256
ASTM D785
kg/cm2 (MPa)
kg·cm/cm (J/m)
-
32000 (3136)
5 (49)
90
Surface Resistivity
ASTM D257
x 1016 Ω
1
Volume Resistivity
Dielectric Strength
Dielectric Constant
ASTM D257
ASTM D149
ASTM D150
x 1014 Ω·m
kV/mm
-
1
-
ASTM D150
-
-
ASTM D495
sec
-
Flexural Modulus
Notched Izod Impact Strength
Rockwell Hardness
Electrical
Dielectric Dissiparation FactorConstan 106 Hz
Arc Resistance
6
10 Hz
The information provided in this data sheet is based on our present state of knowledge and is estimated by
KOLON. This information should not be used as guaranteeing specification limits. KOLON make no
warranty and liability in connection with any use of this information.
KOLON Industries Inc.
KOLON TOWER, 1-23, BYULYANG-DONG, KWACHEN-CITY KYNG GI-DO, KOREA
Tel. 82-2-3677-3580~9 Fax. 82-2-3677-3558