YAGEO CAN4313129200431B

ANTENNA PRODUCTS
WIDE BAND MULTILAYER CERAMIC ANTENNA
FOR 850~950MHz
Product Specification
QUICK REFERENCE DATA
Size
16.5*14*0.9 mm
Working Frequency
850~950MHz
Gain
1.5 dBi Max
VSWR
2 max
Polarization
Linear
Azimuth
Omni-directional
Impedance
50Ω
Operating Temperature
-55~85 o C
Termination
Ni/Sn (Environmentally-Friendly Leadless)
o
433MHz Ceramic
Antenna
260 C, 10 Chip
sec.
Resistance to soldering heats
Special Environmental Concerns- Green Products Design: The foil making process is
using environmentally friendly aqueous solvent technology. Termination is lead free and
packing materials can be re-cycled
Sep, 2005, V3
Print date 05/09/07
15th, Aug, 05
Multilayer Ceramic Antenna
for 433 MHz (small size)
CAN4313 129 200431B
30th, Aug,05
7th, Sep,05
Dennis Liu
spec.doc
C.T.Lee
7th ,Sep, 05
Page 1
sheet 190-1
A4
MULTILAYER CERAMIC ANTENNA (LINEAR POLARIZATION MODE)
FOR 400MHz~500MHz
Product Specification1
QUICK REFERENCE DATA
__________________________________________________________________________
Working Frequency*
400~500MHz
Bandwidth
20 MHz (Min)
Gain
0.5 dBi (Max)
VSWR
3.0 max
Polarization
Linear
Azimuth
Omni-directional
Impedance
50Ω
Operating Temperature
-40~85 o C
Termination
Ni/Sn (Environmentally-Friendly Leadless)
o
Resistance to soldering heat 260 C, 10 sec.
Special Environmental Concerns- Green Products Design: The foil making process is
using environmentally friendly aqueous solvent technology. Termination is lead free and
packing materials can be re-cycled
1. APPLICATION
1
All the technical data and information contained herein are subject to change without prior notice
Print date 05/09/07
15th, Aug, 05
Multilayer Ceramic Antenna
for 433 MHz (small size)
CAN4313 129 200431B
30th, Aug,05
7th, Sep,05
Dennis Liu
spec.doc
C.T.Lee
7th ,Sep, 05
Page 2
sheet 190-2
A4
RFModule
Top Side
40
50 ohm transmission
line
60 mm
Back
Side
Cleanness
Circuits space
Back side all ground plan
( But under antenna should avoid ground )
plane )
Print date 05/09/07
15th, Aug, 05
Multilayer Ceramic Antenna
for 433 MHz (small size)
CAN4313 129 200431B
30th, Aug,05
7th, Sep,05
Dennis Liu
spec.doc
C.T.Lee
7th ,Sep, 05
Page 3
sheet 190-3
A4
2. SOLDER LAND PATTERN FOR ANTENNA
Figure
Dimensions
W
Remark
w
0.85 ± 0.3 mm
Feed Pad
F
4.20 ± 0.3 mm
Feed Pad
F
1
Print date 05/09/07
15th, Aug, 05
Multilayer Ceramic Antenna
for 433 MHz (small size)
CAN4313 129 200431B
30th, Aug,05
7th, Sep,05
Dennis Liu
spec.doc
C.T.Lee
7th ,Sep, 05
Page 4
sheet 190-4
A4
3. MECHANICAL DATA
Figure
Dimension
L
Port
W
4±0.5mm
Feed termination
L
12±0.5mm
Solder termination
T
1.5±0.3mm
W
1
T
4. TEST BOARD DIMENSION FOR S11 (RETURN LOSS) AND
RADIATION PATTERN MEASURNMENT
60 mm
40
50 ohm transmission
FR-4 PCB thickness = 0.8 mm
The length of transmission line = 60 mm ( depends on PCB thickness)
Print date 05/09/07
15th, Aug, 05
Multilayer Ceramic Antenna
for 433 MHz (small size)
CAN4313 129 200431B
30th, Aug,05
7th, Sep,05
Dennis Liu
spec.doc
C.T.Lee
7th ,Sep, 05
Page 5
sheet 190-5
A4
5. S11 RETURN LOSS
Print date 05/09/07
15th, Aug, 05
Multilayer Ceramic Antenna
for 433 MHz (small size)
CAN4313 129 200431B
30th, Aug,05
7th, Sep,05
Dennis Liu
spec.doc
C.T.Lee
7th ,Sep, 05
Page 6
sheet 190-6
A4
RELIABILITY DATA (Reference to IEC Specification)
IEC
IEC
384-10/
CECC 32
100
CLAUSE
6006868-2
TEST
METHOD
TEST
4.4
Mounting
4.5
4.6.1
Visual inspection
and dimension
check
Antenna
4.8
Adhesion
4.9
Bond strength of
plating on end face
PROCEDURE
REQUIREMENTS
The antenna can be
mounted on printedcircuit boards or ceramic
substrates by applying
wave soldering, reflow
soldering (including
vapour phase soldering)
or conductive adhesive
Any applicable method
using × 10 magnification
Central Frequency
at 20 oC
No visible damage
In accordance with
specification (no chip
off 3 mm)
Standard test board
in page 4
A force of 5 N applied
for 10 s to the line
joining the terminations
and in a plane parallel to
the substrate
Mounted in accordance
with CECC 32 100,
paragraph 4.4
No visible damage
Conditions: bending
0.25 mm at a rate of
1mm/s, radius jig. 340
mm,1 mm warp on FR4
board of 90 mm length
No visible damage
No visible damage
Print date 05/09/07
15th, Aug, 05
Multilayer Ceramic Antenna
for 433 MHz (small size)
CAN4313 129 200431B
30th, Aug,05
7th, Sep,05
Dennis Liu
spec.doc
C.T.Lee
7th ,Sep, 05
Page 7
sheet 190-7
A4
IEC
IEC
384-10/
CECC 32
100
CLAUSE
6006868-2
TEST
METHOD
4.10
Tb
TEST
Resistance to
soldering heat
PROCEDURE
REQUIREMENTS
260 ± 5 °C for 10 ± 0.5
s in a static solder bath
The terminations
shall be well tinned
after recovery and
Central Freq. Change
± 6%
Resistance to
leaching
4.11
Ta
Solderability
260 ± 5 °C for 30 ± 1 s
in a static solder bath
Using visual
enlargement of × 10,
dissolution of the
termination shall not
exceed 10%
Zero hour test, and test
The termination must
after storage (20 to 24
be well tinned, at
months) in original
least 75% is well
atmosphere; un-mounted tinned at termination
chips completely
immersed for 2 ± 0.5 s in
235 ± 5°C.
Print date 05/09/07
15th, Aug, 05
Multilayer Ceramic Antenna
for 433 MHz (small size)
CAN4313 129 200431B
30th, Aug,05
7th, Sep,05
Dennis Liu
spec.doc
C.T.Lee
7th ,Sep, 05
Page 8
sheet 190-8
A4
ORDERING INFORMATION:
The antenna may be ordered by using the ordering code. These code numbers can be
determined by the following rules:
CAN43 13 1 29 20 043 1B
F
C M S T A T
F. Family Code
CAN43 = Antenna
C. Packing Type Code
13 = Bulk
M. Materials Code
1 = High Frequency Material
S. Size Code
29 =12* 4 * 1.5 mm
T. Tolerance
20 = 20M Hz Band Width
A. Working Frequency
043 = 400~500MHz
CAN43
Product
CAN43=
Antenna
13
Packing
type
Bulk
CAN4311129200431B (Clear Text Code Example)
1
29
20
043
Material
Size
Type
Working
Frequency
LTCC
29=12*4mm 20=
043=433MHz
material
20MHz
1
Quantities
1= 1K pcs
B
Packing
Bulking
packing
Print date 05/09/07
15th, Aug, 05
Multilayer Ceramic Antenna
for 433 MHz (small size)
CAN4313 129 200431B
30th, Aug,05
7th, Sep,05
Dennis Liu
spec.doc
C.T.Lee
7th ,Sep, 05
Page 9
sheet 190-9
A4
Revision Control:
Revision
Date
th
Content
Remark
1
15 , Aug. 2005
New Issued
2
30th, Aug. 2005
Modification of end-termination’s appearance
3
th
7 , Sep. 2005
Modification of 12nc and packing type
Print date 05/09/07
15th, Aug, 05
Multilayer Ceramic Antenna
for 433 MHz (small size)
CAN4313 129 200431B
30th, Aug,05
7th, Sep,05
Dennis Liu
spec.doc
C.T.Lee
7th ,Sep, 05
Page 10
sheet 190-10
A4