Package Compliance Report

Super 247
RoHS Compliance Document
Contents:
1. Composition
2. Tin Whisker Report
The information contained in this document is provided without any warranty, either expressed or implied, and IR
specifically disclaims any and all liability, including but not limited to consequential or indirect damages.
July 2014
SUPER-247
Component
Material
Name
Material
Mass
(g)
Element
Name
Composition
Si
SiO2
Epoxy
Other
Cu
Fe
Sn
Ag
Sb
Al
Ni
Sn
Total Weight
(g)
Chip
Silicon
0.05530
Encapsulant
Epoxy Resin
0.81510
Lead Frame
Copper
5.35810
Die Attach
J-Alloy
0.02730
Wire Bond
Aluminum
0.04780
Lead Finish
Matte Tin
over Nickel*
0.07060
CAS #
Substance
Mass (g)
7440-21-3
7631-86-9
90598-46-2
7440-50-8
7439-89-6
7439-92-1
7440-22-4
7440-36-0
7429-90-5
7440-02-0
7440-31-5
0.05530
0.66267
0.06521
0.08722
5.33131
0.02679
0.01774
0.00683
0.00273
0.04780
0.00988
0.06072
Material
Analysis
Weight
(%)
100%
81%
8%
11%
100%
0%
65%
25%
10%
100%
14%
86%
% of Total
Weight
0.9%
10.4%
1.0%
1.4%
83.6%
0.4%
0.3%
0.1%
0.0%
0.7%
0.2%
1.0%
6.37420
*Tin whisker mitigation strategy is nickel under-plate.
This part is compliant with EU Directive 2011/65/EU (RoHS Directive) and does not contain lead, mercury,
cadmium (0.01%), hexavalent chromium, PBB or PBDE in concentrations greater than 0.1%, except as
permitted by Annex (7).
The information contained in this document is provided without any warranty, either expressed or implied, and IR specifically
disclaims any and all liability, including but not limited to consequential or indirect damages.
1
July 2014
SUPER-247
Test Definition
Room
Temperature
Humidity
Storage
Temperature
Humidity
Unbiased
Inspection
Total
Interval Class
Duration
1 and 2
Class 1 and 2
Products
Products
Test Conditions
Maximum
Whisker
Length
(µm)
30± 2°C/60± 3% RH
1000 hours
4000 hours
20
55± 3°C/85± 3% RH
1000 hours
4000 hours
20
-40 to 55°C to 80 to 95°C,
500 cycles
1500 cycles
air to air, 10 min soak,
approx 3
cycles
/hours
Tin Whisker testing per JESD201,
Environmental Acceptance Requirements for
Tin Whisker Susceptibility of Tin and Tin Alloy Surface Finish
Temperature
Cycling
45
Tin Whisker Results (number of failing whiskers)
Test
Room Temperature
Humidity Storage
Temperature
Humidity
Unbiase
Test
d
Temperature Cycling
1000 Hours
2000 Hours
3000 Hours
4000 Hours
0/24
0/24
0/24
0/24
0/24
0/24
0/24
0/24
500 Cycles
1000 Cycles
0/24
0/24
1500 Cycles
0/24
The information contained in this document is provided without any warranty, either expressed or implied, and IR specifically
disclaims any and all liability, including but not limited to consequential or indirect damages.
2
July 2014