SANYO OS-CON25SVP33M

OS-CON DATA SHEET
No.OS02N-DFSVP047
OS-CON 25SVP33M
Frequency (kHz)
Impedance (ohm)
ESR (ohm)
0.12
38.917
0.361
0.5
9.405
0.145
1
4.720
0.110
10
0.496
0.060
100
0.067
0.026
500
0.020
0.018
1000
0.018
0.016
5000
0.085
0.018
10000
0.163
0.024
Frequency characteristics
1000
Impedance (ohm)
ESR (ohm)
ESR, Impedance (ohm)
100
10
1
0.1
0.01
0.001
0.1
1
10
100
1000
10000
Frequency (kHz)
Measureing equipment: HP4194A
Test fixture: HP16047C
Measuring position: root of leads
OS Engineering Department, OS-CON Control Department
Saga SANYO Industries Co., Ltd.
n = 3p.(Ave.)
Room temperature
OS-CON DATA SHEET
SVP series
Test item
Endurance
(After V.P.S test)
Test temperature
105 deg.C
Model
Applied voltage
20V
Lot No.
25SVP33M
0O1002541
Tangent of loss angle (120Hz)
Change in capacitance (120Hz)
Tangent of loss angle
20
Percent delta [%]
10
0
-10
-20
-30
-40
2000
0
Time[h]
ESR (100kHz)
Leakage current (25V 60s)
10000
100
90
80
70
60
50
40
30
20
10
0
1000
100
10
1
0.1
0.01
0
2000
Time[h]
Note:
2000
Time[h]
Leakage current(µA)
ESR(mohm)
0
0.15
0.14
0.13
0.12
0.11
0.1
0.09
0.08
0.07
0.06
0.05
0.04
0.03
0.02
0.01
0
0
2000
Time[h]
n =30p.
V.P.S test conditions : 230deg.C×75s×2times
(V.P.S = Vapor Phase Soldering method)
Start on November 1, 2000
Executed by M. Koyama
End on January 23, 2001
Drawn by M. Kimura
No.OS02D-DESVP047
OS Engineering Department, OS-CON Control Department, Saga SANYO Industries Co., Ltd.
OS-CON DATA SHEET
SVP series
Test item
Damp heat (Steady state)
(After V.P.S test)
Test temperature
60 deg.C
Model
Test humidity
90% RH
Lot No.
25SVP33M
0O1002541
Change in capacitance (120Hz)
Tangent of loss angle (120Hz)
Tangent of loss angle
20
Percent delta (%)
10
0
-10
-20
-30
-40
1000
0
Time[h]
ESR (100kHz)
Leakage current (25V 60s)
100
90
80
70
60
50
40
30
20
10
0
10000
1000
100
10
1
0.1
0.01
0
1000
Time[h]
Note:
1000
Time[h]
Leakage current(µA)
ESR(mohm)
0
0.15
0.14
0.13
0.12
0.11
0.1
0.09
0.08
0.07
0.06
0.05
0.04
0.03
0.02
0.01
0
0
1000
Time[h]
n =20p.
V.P.S test conditions : 230deg.C×75s×2times
(V.P.S = Vapor Phase Soldering method)
Start on November 1, 2000
Executed by M. Koyama
End on December 13, 2000
Drawn by M. Kimura
No.OS02D-DHSVP047
OS Engineering Department, OS-CON Control Department, Saga SANYO Industries Co., Ltd.